Recently got 2 bronze head march 809 pumps, should I worry about galvanic corrosion if I put stainless camlocks on these?

My other option would be polypropylene cam locks.

Thanks,
 
Without even reaching for the tables I'll say it's not a problem as I have had stainless 3A sanitary fittings on the bronze volutes of my March pumps for years and have not noticed any corrosion.
 
Without even reaching for the tables I'll say it's not a problem as I have had stainless 3A sanitary fittings on the bronze volutes of my March pumps for years and have not noticed any corrosion.

Thank you, that makes me very happy:tank:
 