Well-Known Member
Yeah, they were SS. My welder had them cherry red for a loooonnnnggg time. I told him how screwed up it is, and he told me he would "reweld it with more gas this time to stabilize the chromium." He had prep sanded it with a really old jacked up pad...probably was contaminated with steel from his kid's car project.