So after i went through all that trouble of getting my kegs welded, and having to clean them up, it turns out i have a pin hole leak in one of the welds..

so what should i do? I really dont want to make a big fuss about it..

suggestions?
 
If your welder missed a hole then that is not his problem but if you asked him to weld all the leaks and leak test then he should be glad to fix it. He most likely will fix it no charge if he made reasonable money on the job the first time. I would at least show it to him. :) Most welders like to please.
 
Its a two party epoxy. mix the grey and white 50/50, spread it on, wait 24 hours. Its great stuff! You could also braise the hole with a rod and a mini propane/mapp gas torch.
 
Ugh, sorry to see that. Is JB Weld food safe? The problem is adhesion, especially to SS. I have never used JB Weld on SS, nor for food applications. I really don't know what to suggest, other than having a different welder fix the weld.

Ok they claim it is non-toxic and will bond fine to Steel (I didn't specifically see SS though).
 
If you don't allow a business to correct a problem then the business is not bad, you just might be a bad customer.

I used JB weld on a corny with a pinhole leak. No problems. YMMV.
 
Why don't you want to take the keggle back and get it fixed by the welder?
 
Come on guys, this is brewing and we should not use any bunch of chemicals (JB Weld) that will leach into the brew. I suggest finding a good quality weld shop that knows how to make proper welds on stainless with shielding gas on both sides of the weld. Mickey mousing things is just BAD.
 
Silversolder the thing! If you have sweated copper you have 1/3 the materials you need. (note, I havn't silver soldered yet. I plan on doing it soon... as soon as I have money for the !@#$!@#$!@#$ solder. It's not cheap, but it's SWEET!!!)
 
Come on guys, this is brewing and we should not use any bunch of chemicals (JB Weld) that will leach into the brew. I suggest finding a good quality weld shop that knows how to make proper welds on stainless with shielding gas on both sides of the weld. Mickey mousing things is just BAD.

My understanding is that once cured there is no leeching and no toxicity. Your point is well taken though; I got rid of all my Teflon pans years ago for the same reason. Here are the MSDS sheets for the two part epoxy.


http://jbweld.net/techinfo/JB Weld-Epoxy Steel Hardener-Overnight-48008.pdf

http://jbweld.net/techinfo/JB Weld-Epoxy Steel Resin-Overnight-48009.pdf
 
If it's just a pin hole leak, then you can "ping" it.
Use a sharp tipped punch. Set it just to the side of the pin hole and hit the punch, with a hammer, back toward the pin hole. It may take a couple of hits to seal the leak.
 
This is why I go weldless... $16 from morebeer and it is done without leaks and fuss. I know I know, some of yall swear by welding... but I converted 3 kegs for under $50 and they don't leak, took all of 15 minutes!
 
ok, i havent gotten this fixed yet.. but i was looking at using some lead free solder on the hole.. it has a melting point of 450f.. would that work?
 
JB weld might as well be steel. Its so hard it can be machined. I used it once to plug a pinhole Gasoline leak, while it was leaking!

Id use it and fuggedaboutit
 
I'd probably go the silver solder route if I already had the propane torch, otherwise JB weld, that stuff can fix an engine block.

As for silicone, it can stand fairly high temps
 
is that silicone hi temp? where can i find stuff like that?

Go here: http://www.mcmaster.com/ search for item# 74515A32

Dow Corning Silicone Sealant #736

"736 Heat Resistant— Excellent for sealing and encasing heating elements in adhesive (potting), aerospace gasketing, insulation, and as a protective coating. Begins to harden in 17 minutes. Temp. range is -85° to +500° F. Complies with USDA and FDA Regulation 21 CFR 177.2600 covering indirect food contact. NSF-51 certified for use with food equipment materials. UL listed. Meets MIL-A-46016, Group I, Type I. "
 